PEEK Plastic injection molding parts components case study
Customer Profile: It is a company in the electronics industry, so the anti-static measures required for Plastic injection molding parts components PEEK electronic product
Static electricity has great damage and influence on electronic products. Circuits are quite sensitive to electrostatic high voltage. When a person or object with static electricity touches these components, electrostatic discharge will occur, resulting in damage to components or abnormal operation. Therefore, prevent static electricity. It is the key that the electronics industry cannot ignore.
Plastic injection molding parts Name: Standardized Lower Contact Floating Plate M
Plastic injection molding parts components material: Peek anti-static
Plastic injection molding parts components Difficulties: Filling Dissatisfaction and Surface Resistance Anti-static Requirements
The net weight of the product : 0.886g*2
Peek engineering plastic material is characterized by fast crystallization and slow flow rate, which is easy to cause the phenomenon of unsatisfactory product filling.

We can see that the pins of PEEK products are not filled and the surface of the product is uneven by comparing with qualified plastic injection molding parts components.

There are several reasons for this:
1. The physical temperature of PEEK is not reached, and the injection temperature can be appropriately increased
2. There are additives in the PEEK material itself
3. The product itself is too thick and it is not easy to fill it completely. The product can be re-evaluated by adjusting the shape of the product
4. The injection pressure is small and the holding pressure is not enough. The injection machine debugging personnel should appropriately increase the injection pressure and increase the holding time.
5. In view of the small flow channel of the mold itself, it is obvious that we expand the mold flow channel to facilitate the smooth entry of PEEK plastic into the cavity

This product is different from ordinary PEEK. It needs to meet the electrostatic value standard required by the customer. The customer's requirement for the surface resistance of the product is to reach the sixth power of 10 to the eighth power of ten.
According to customer requirements, we have special test equipment.
https://www.yizemould.com/newsdetail-896.html
saefeyiz
Recently Posted
-
ABS 30% anti-static thermoplastics injection molding
May 4, 2023Case Study: Co-Molding 5 Products with One Set for ABS 30% anti-static thermoplastics injection moldingIntroduction:Our client required the production of five different ABS 30% anti-static thermoplastics injection molding, all to be co-molded using only one set of molds. The parts needed to meet specific surface quality requirements, with different areas designated as either A-Level or B-Level surfaces.A-Level Surface ReRead More -
Solenoid valve housings made of PBT 30% Engineering Plastics injection molding
May 4, 2023Case study of a problem that manufactures solenoid valve housings made of PBT 30% Engineering Plastics injection molding.The company found the following problems in the PBT 30% Engineering Plastics injection molding:1. The red circle has burrs, with a step difference of about 0.05;2. The appearance of the red circle is uneven and the knife lines are serious;3. The red circle has fiber marks and serious air trapping. ThisRead More -
Case study Amphenol with LCP E130i Thermoplastics Precision Molded V-0 Material
May 4, 2023Introduction: Amphenol is a leading manufacturer of high-quality electronic connectors and interconnects systems. When Amphenol approached us to produce molded parts for their products using LCP E130i Thermoplastics Precision Molded V-0 material, we knew we had a challenging task ahead of us. This material is known for its high strength and excellent flame retardant properties, but it also has specific requirementsRead More -
About SMT high precision connector injection
February 6, 2023With the development of technology, many objects are now becoming lighter, smaller, and smarter, because they are easy to carry and easy to use, and the connector industry is no exception. Under the current trend of smaller and smaller connectors, it also poses a huge challenge to the material of the connector. Under this trend, high-temperature nylon and LCP emerged as the times require, and they shine in the field of SRead More